• Bomba la Tittanium na Nyenzo za Tube:Titanium safi (CP) na karatasi ya aloi ya Titanium,Daraja la 1, la 2, la 5, la 5, la 7 na la 9.
• Aina: Mirija isiyo na mshono, Mirija ya Kuchomezwa, Coil Tube, bomba la kubadilisha joto, U-Bend Tube, Capillary Tube
• Kipimo:OD: 3~1500mm, WT: 0.2~25mm: Urefu: ≤19000mm
• Masharti:Rolling, kulehemu, Machining
• Viwango:ASTM B338, ASTM B337, ASTM B861, ASTM B862 n.k.
• Maombi:Shell na exchanger joto tube, condenser, evaporator, bomba,Vifaa vya kusafisha maji ya bahari, Rafu ya Baiskeli, bomba la shinikizo la baharini, bomba la shinikizo la kuchimba mafuta,
Aloi ya Titanium Nyenzo Jina la Kawaida | ||
Gr1 | UNS R50250 | CP-Ti |
Gr2 | UNS R50400 | CP-Ti |
Gr4 | UNS R50700 | CP-Ti |
Gr7 | UNS R52400 | Ti-0.20Pd |
G9 | UNS R56320 | Ti-3AL-2.5V |
G11 | UNS R52250 | Ti-0.15Pd |
G12 | UNS R53400 | Ti-0.3Mo-0.8Ni |
G16 | UNS R52402 | Ti-0.05Pd |
G23 | UNS R56407 | Ti-6Al-4V ELI |
Bomba la Titanium na Mirija:Mrija usio na mshono wa titani huchakatwa kwa kuvunjika kwa ingoti ya titani, na kutolewa kwenye billet ya mirija ya titani.Kisha toa mirija ya titani kwa ukubwa ufaao kwa mfululizo wa michakato kama vile kuviringisha, kuchuna, kuchuna na kusaga teknolojia.
Titanium svetsade tube ni kwa kuchagua unene kufaa ya ubora wa juu baridi akavingirisha titan sahani, baada ya mchakato wa flatten, kukata na kuosha, kisha akavingirisha juu ya sahani titanium katika neli, kulehemu kwa zima moja kwa moja vifaa vya kulehemu.Vifaa vyetu vya juu vya kulehemu vilihakikisha ubora wa kulehemu.Hatimaye kusaidia kuzalisha ubora bora wa titanium tube.
Daraja | Muundo wa kemikali, asilimia ya uzito (%) | ||||||||||||
C (≤) | O (≤) | N (≤) | H (≤) | Fe (≤) | Al | V | Pd | Ru | Ni | Mo | Vipengele Vingine Max.kila mmoja | Vipengele Vingine Max.jumla | |
Gr1 | 0.08 | 0.18 | 0.03 | 0.015 | 0.20 | - | - | - | - | - | - | 0.1 | 0.4 |
Gr2 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | - | - | - | - | - | - | 0.1 | 0.4 |
Gr4 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | - | - | - | - | - | - | 0.1 | 0.4 |
Gr5 | 0.08 | 0.20 | 0.05 | 0.015 | 0.40 | 5.56.75 | 3.5 4.5 | - | - | - | - | 0.1 | 0.4 |
Gr7 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | - | - | 0.12 0.25 | - | 0.12 0.25 | - | 0.1 | 0.4 |
Gr9 | 0.08 | 0.15 | 0.03 | 0.015 | 0.25 | 2.5 3.5 | 2.0 3.0 | - | - | - | - | 0.1 | 0.4 |
Gr11 | 0.08 | 0.18 | 0.03 | 0.15 | 0.2 | - | - | 0.12 0.25 | - | - | - | 0.1 | 0.4 |
Gr12 | 0.08 | 0.25 | 0.03 | 0.15 | 0.3 | - | - | - | - | 0.6 0.9 | 0.2 0.4 | 0.1 | 0.4 |
Gr16 | 0.08 | 0.25 | 0.03 | 0.15 | 0.3 | - | - | 0.04 0.08 | - | - | - | 0.1 | 0.4 |
Gr23 | 0.08 | 0.13 | 0.03 | 0.125 | 0.25 | 5.5 6.5 | 3.5 4.5 | - | - | - | - | 0.1 | 0.1 |
Daraja | Tabia za kimwili | |||||
Nguvu ya mkazo Dak | Nguvu ya mavunoKiwango cha chini (0.2%, punguzo) | Elongation katika 4D Kiwango cha chini (%) | Kupunguza eneo Kiwango cha chini (%) | |||
ksi | MPa | ksi | MPa | |||
Gr1 | 35 | 240 | 20 | 138 | 24 | 30 |
Gr2 | 50 | 345 | 40 | 275 | 20 | 30 |
Gr4 | 80 | 550 | 70 | 483 | 15 | 25 |
Gr5 | 130 | 895 | 120 | 828 | 10 | 25 |
Gr7 | 50 | 345 | 40 | 275 | 20 | 30 |
Gr9 | 90 | 620 | 70 | 483 | 15 | 25 |
Gr11 | 35 | 240 | 20 | 138 | 24 | 30 |
Gr12 | 70 | 483 | 50 | 345 | 18 | 25 |
Gr16 | 50 | 345 | 40 | 275 | 20 | 30 |
Gr23 | 120 | 828 | 110 | 759 | 10 | 15 |
•Daraja la 1: Titanium Safi, nguvu ya chini kiasi na ductility ya juu.
•Daraja la 2: Titanium safi inayotumika zaidi.Mchanganyiko bora wa nguvu
•Daraja la 3: Titanium yenye nguvu nyingi, inayotumika kwa sahani za Matrix katika ganda na vibadilisha joto vya mirija
•Daraja la 5: Aloi ya titani iliyotengenezwa zaidi.Nguvu ya juu sana.upinzani wa joto la juu.
•Daraja la 7: Upinzani bora wa kutu katika kupunguza na mazingira ya vioksidishaji.
•Daraja la 9: Nguvu ya juu sana na upinzani wa kutu.
•Daraja la 12: Ustahimilivu bora wa joto kuliko Titanium safi.Maombi ya darasa la 7 na 11.
•Daraja la 23: Titanium-6Aluminium-4Vanadium ELI (Idara ya Ziada ya Chini) Aloi ya kupandikiza kwa upasuaji.