Titanium Capillary Tube:Kutokana na aloi za Titanium elongation ya titani ya usafi inaweza kuwa hadi 50-60%, na kupunguza eneo inaweza kuwa hadi 70-80%.Hiyo inafanya uzalishaji wa titanium capillary tube.Kuunda na kuviringisha ingoti za titani zinazoyeyuka kwenye bili za mirija, kisha unyooshe billet ya bomba kwa mara kadhaa hadi bomba la kapilari la titani litengenezwe.Kutokana na utangamano mzuri na mwili wa binadamu na upinzani wa kutu, tube ya capillary ya titani hutumiwa sana katika sekta ya matibabu, ikiwa ni pamoja na vipandikizi vya mwili wa binadamu, vifaa vya matibabu sehemu za ndani za usahihi, nk.
• Nyenzo za Mirija ya Kapilari ya Tittanium: Titanium Safi,Grade1,Grade 2,Grade 5,Grade 5,Grade7,Grade9,Grade11,Grade12,Grade 16,Grade23 ect.
• Vipimo:OD: 0.2 ~ 8mm, WT: 0.015 ~ 0.5mm, Urefu≤6000mm
• Viwango:ASTM B338, ASTM B337, ASTM B861, ASTM B862 n.k.
Aloi ya Titanium Nyenzo Jina la Kawaida | ||
Gr1 | UNS R50250 | CP-Ti |
Gr2 | UNS R50400 | CP-Ti |
Gr4 | UNS R50700 | CP-Ti |
Gr7 | UNS R52400 | Ti-0.20Pd |
G9 | UNS R56320 | Ti-3AL-2.5V |
G11 | UNS R52250 | Ti-0.15Pd |
G12 | UNS R53400 | Ti-0.3Mo-0.8Ni |
G16 | UNS R52402 | Ti-0.05Pd |
G23 | UNS R56407 | Ti-6Al-4V ELI |
Daraja | Muundo wa kemikali, asilimia ya uzito (%) | ||||||||||||
C (≤) | O (≤) | N (≤) | H (≤) | Fe (≤) | Al | V | Pd | Ru | Ni | Mo | Vipengele Vingine Max.kila mmoja | Vipengele Vingine Max.jumla | |
Gr1 | 0.08 | 0.18 | 0.03 | 0.015 | 0.20 | - | - | - | - | - | - | 0.1 | 0.4 |
Gr2 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | - | - | - | - | - | - | 0.1 | 0.4 |
Gr4 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | - | - | - | - | - | - | 0.1 | 0.4 |
Gr5 | 0.08 | 0.20 | 0.05 | 0.015 | 0.40 | 5.56.75 | 3.5 4.5 | - | - | - | - | 0.1 | 0.4 |
Gr7 | 0.08 | 0.25 | 0.03 | 0.015 | 0.30 | - | - | 0.12 0.25 | - | 0.12 0.25 | - | 0.1 | 0.4 |
Gr9 | 0.08 | 0.15 | 0.03 | 0.015 | 0.25 | 2.5 3.5 | 2.0 3.0 | - | - | - | - | 0.1 | 0.4 |
Gr11 | 0.08 | 0.18 | 0.03 | 0.15 | 0.2 | - | - | 0.12 0.25 | - | - | - | 0.1 | 0.4 |
Gr12 | 0.08 | 0.25 | 0.03 | 0.15 | 0.3 | - | - | - | - | 0.6 0.9 | 0.2 0.4 | 0.1 | 0.4 |
Gr16 | 0.08 | 0.25 | 0.03 | 0.15 | 0.3 | - | - | 0.04 0.08 | - | - | - | 0.1 | 0.4 |
Gr23 | 0.08 | 0.13 | 0.03 | 0.125 | 0.25 | 5.5 6.5 | 3.5 4.5 | - | - | - | - | 0.1 | 0.1 |
Daraja | Tabia za kimwili | |||||
Nguvu ya mkazo Dak | Nguvu ya mavuno Kiwango cha chini (0.2%, punguzo) | Elongation katika 4D Kiwango cha chini (%) | Kupunguza eneo Kiwango cha chini (%) | |||
ksi | MPa | ksi | MPa | |||
Gr1 | 35 | 240 | 20 | 138 | 24 | 30 |
Gr2 | 50 | 345 | 40 | 275 | 20 | 30 |
Gr4 | 80 | 550 | 70 | 483 | 15 | 25 |
Gr5 | 130 | 895 | 120 | 828 | 10 | 25 |
Gr7 | 50 | 345 | 40 | 275 | 20 | 30 |
Gr9 | 90 | 620 | 70 | 483 | 15 | 25 |
Gr11 | 35 | 240 | 20 | 138 | 24 | 30 |
Gr12 | 70 | 483 | 50 | 345 | 18 | 25 |
Gr16 | 50 | 345 | 40 | 275 | 20 | 30 |
Gr23 | 120 | 828 | 110 | 759 | 10 | 15 |
•Daraja la 1:Titanium safi, nguvu kidogo na ductility ya juu.
• Daraja la 2:Titanium safi inayotumika zaidi.Mchanganyiko bora wa nguvu
• Daraja la 3:Titanium yenye nguvu ya juu, inayotumika kwa sahani za Matrix kwenye ganda, vibadilisha joto vya mirija
• Daraja la 5:Aloi ya titanium iliyotengenezwa zaidi. Nguvu ya juu sana na upinzani wa joto.
• Daraja la 7:Upinzani bora wa kutu katika kupunguza na mazingira ya vioksidishaji.
• Daraja la 9:Nguvu ya juu sana na upinzani wa kutu.
• Daraja la 12:Upinzani bora wa joto kuliko Titanium safi.kutumika kwa darasa la 7 na 11.
•Daraja la 23:Titanium-6Aluminium-4Vanadium ELI (Mwisho wa Kinga ya Ziada wa Chini) kwa uwekaji wa kupandikiza kwa upasuaji.